551PF Colorpro series Plastisol inks for colour mixing system PANTONE© using 11 standard colorful colors (including black and white). Colorpro series is suitable for both light and dark fabrics. Very easy to prepare. Simply select the desired color from PANTONE Color Formula Guide and locate the appropriate formula in colorpro series Mixing Guide. After mixing plastizolya paint , if the paint is not enough bright, add 5% -20% of 551PF color Booster to achieve brightness color.

551 COLORPRO SERIES "PF" YELLOW GS
551 COLORPRO SERIES "PF" YELLOW RS
551 COLORPRO SERIES "PF" RED YS
551 COLORPRO SERIES "PF" RED BS
551 COLORPRO SERIES "PF" BLUE GS
551 COLORPRO SERIES "PF" BLUE RS
551 COLORPRO SERIES "PF" FLO MAGENTA
551 COLORPRO SERIES "PF" VIOLET
551 COLORPRO SERIES "PF" GREEN "BS"
551 COLORPRO SERIES "PF" WHITE
551 COLORPRO SERIES "PF" BLACK
551 "PF" BASE (COLORPRO SERIES)

TECHNICAL DETAILS

Drying: paint starts drying on the surface at 240 ° F (116 ° C), fully harden, when the whole paint layer reaches a temperature 320 ° F. (160 ° C). For lighter colors may require more the time to reach this temperature.The paint starts drying on surface at 240 ° F (116 ° C).

Thermotransfer (cold peel): 250°F (121°C), 1.5 min. Possible more short-term option, but when a higher temperature (about 30 sec, 325°F /163°C).

Transfers, hot split: for transfers, hot split colorpro series series 951.

Blanket: 2000 Green or TR Enviro Blend Series.

Mesh: for direct printing you can use 40-305/inch (16-122 cm) polyester. For thermotransfer more suited 80-125 per inch (32-50 cm).

Raquel: medium Durometer

Emulsija: any emulsion or capillary film, compatible with plastisol inks is recommended.

Modification of the paint: to obtain the desired consistency, can be used diluent 502 Reducer. A certain amount of diluent will give a print on water-based. The only drawback is that with increasing the quantities used, the plastisol loses some elasticity and resistance to friction. The use of an excessive amount of can to increase drying time.

ATTENTION

Always check the finished prints for color accuracy, vysypanie adhesion and the desired appearance before the full manufacturing cycle.

Made in Canada.

Plastisol inks - General information


Drying conditions plestezolevy paints

THE THICKNESS OF THE PAINT LAYER

When direct printing on the product, the drying is best to start with 1.5 min, 320ºF (160ºC). Large image nylon sports the form may require 2.5 minutes and 340ºF (173ºC). The greater the volume and/or the thickness of the plastisol on the product, the more time and/or higher the temperature required.

PAINT COLOR

In the drying time of bright colors (white, gold, and so on) under infrared light or infrared conveyor dryers, you may need reducing the speed of the tape. The light color can reflect infrared the radiation. In the drying oven with forced ventilation, the color is not so important, but in any case, special care should be taken during the process drying of red and black colors!

ACHIEVING HIGH COVERAGE ON DARK SUBSTRATES


Ink ability (opacity) is directly related to the thickness of the imprint, type fabric and drying. For optimal results:

Control the thickness of the right choice of grid size is 50-60 per inch (20-24 cm), type squeegee (medium hardness), and the viscosity of the paint affect the quality result. The viscosity of the ink is a defining moment in the application of the imprint on the product. Tissue type and pressure of the squeegee affect the penetration of dye in fiber fabric. The thicker the print, the higher the opacity. Often achieve a good result on a multi-colour drawings, is used the white background. To get in shape persistent bright rooms, often use a grid 30/inch (12 cm).


  1. Fabric type for optimal results on dark polyester tissues, use temperature to 325º F (163º C) or below. Remember that if this temperature is below the one at which you usually work, increase the dwell time in the dryer.
  2. Use White (wonderful white) as the substrate. This will eliminate or reduce the problem of migration of the dyes on polyester in most cases.
  3. Check the total melting or solidification - remember! When the temperature of the imprint reaches 310º F - 330º F (154º C - 165º C), the total solidification is completed. Plastisol ink thermoplastic (become soft when heated), and any checks hardening should be carried out when the print room temperature. If the fingerprint of the crack when bent, drying was performed wrong. In cases where the paint has been added too much thinner, paint will not harden, regardless of time and temperature the drying.

a) to check the quality of drying plastisol, better just pull and stretch the product. Any cracks suggests that image Nedosekina. Make sure that the whole image was the same thickness of paint (on clearance), because the thicker areas dried more slowly. Rubbing and scratching is also a good means of verification the quality of work done.

b) Good test - resistance the washing. If the paint was Nedosekina, the mechanical fixation of the fibers will be weak and the resistance to washing is bad.

C) Migration of pigment to the surface is often confused with curing plastisol. In most if you can